Determining the influence of the microstructure and phase composition of glass-metal-ceramic coatings on their basic physical-technical properties
DOI:
https://doi.org/10.15587/1729-4061.2021.244004Keywords:
heat-resistant coating, coating microstructure, phase composition, heat-resistant alloys, gas corrosion, glass-metal-ceramic coatingAbstract
Given the development of new heat-resistant nickel alloys that operate at temperatures up to 1,250 °C, as well as the introduction of additive technologies for the production of various parts, it is a relevant task to devise new compositions of highly heat-resistant coatings.
Determining the influence of the phase composition of glass-metal-ceramic coatings on its basic properties could improve the effectiveness of protecting those parts that operate under extreme conditions. Therefore, it is promising to conduct a study aimed at establishing the relationship between the microstructure and phase composition of glass-metal-ceramic coatings and the main physical-technical characteristics.
This study's results have established that the most high-quality coatings were obtained on the basis of non-crystallizing glass. Such glass is characterized by a temperature coefficient of linear expansion of 92·10-7 degrees-1, a glass transition temperature of 625 °C, and surface tension of 260·10-3 N/m at 850 °C. These properties contribute to the formation of a defect-free coating, providing uniform spreading and high-quality adhesion to the substrate.
The resulting optimal coating is characterized by the adhesion strength of 98 %, the thermal resistance (mode 950↔20 °C) of 50 cycles, and the high heat resistance (a weight gain after 100 h in the temperature range of 1,000‒1,050 °C) of 0.03 g/m2·h.
Coatings with a minimum amount of glass bonding are distinguished by uniformity and high quality. The optimal ratio of phases "glass:metal-ceramic composition" is 10:90.
The structure of the recommended coating is uniform, characterized by the homogeneous distribution of components, the absence of cracks, visible defects, and high quality. The phase composition of the coating after firing is represented by crystals of metallic nickel and silicon, as well as a small amount of residual glass phase.
References
- Elizarova, Y. A., Zakharov, A. I. (2021). High-Temperature Functional Protective Coatings. Refractories and Industrial Ceramics, 61 (5), 592–599. doi: https://doi.org/10.1007/s11148-021-00525-4
- Chen, M., Zhu, S., Wang, F. (2015). High temperature oxidation of NiCrAlY, nanocrystalline and enamel-metal nano-composite coatings under thermal shock. Corrosion Science, 100, 556–565. doi: https://doi.org/10.1016/j.corsci.2015.08.033
- Solntsev, S. S., Rozenenkova, V. A. (2006). Glass protective process coatings for heat treatment of steels and alloys. Glass and Ceramics, 63 (11-12), 386–390. doi: https://doi.org/10.1007/s10717-006-0130-9
- Denisova, V. S. (2018). High-temperature glass-ceramic coatings to protect nickel alloys formed at near-operating temperatures. Space Engineering and Technology, 2 (21), 24–32. Available at: https://www.energia.ru/ktt/archive/2018/02-2018/02-2018.pdf
- Abraimov, N. V., Eliseyev, Yu. S., Shkretov, Yu. P., Teryokhin, A. M. (2008). Advanced Technologies for the Protection of Turbine Blades Against Gas Corrosion. Polyot, 3, 17–24. Available at: http://www.mashin.ru/files/pol_03_1_60.pdf
- Majumdar, A., Jana, S. (2001). Glass and glass-ceramic coatings, versatile materials for industrial and engineering applications. Bulletin of Materials Science, 24 (1), 69–77. doi: https://doi.org/10.1007/bf02704843
- Chen, K., Chen, M., Wang, Q., Zhu, S., Wang, F. (2017). Micro-alloys precipitation in NiO- and CoO-bearing enamel coatings and their effect on adherence of enamel/steel. International Journal of Applied Glass Science, 9 (1), 70–84. doi: https://doi.org/10.1111/ijag.12284
- Solntsev, S. S., Denisova, V. S. (2019). Reaction-Cured Composite Coatings and Glasses. Glass and Ceramics, 76 (3-4), 126–130. doi: https://doi.org/10.1007/s10717-019-00148-9
- Bragina, L. L., Savvova, O. V. (2009). Structural particulars and formation mechanisms of glass coatings belonging to the system Na2O-B2O3-ZnO-TiО2-SiО2. Glass and Ceramics, 66 (7-8), 262–264. doi: https://doi.org/10.1007/s10717-009-9179-6
- Wang, M., Li, X., Su, D., Ji, H., Tang, H., Zhao, Z., He, J. (2016). Effect of glass phase content on structure and properties of gradient MoSi2 -BaO-Al2O3 - SiO2 coating for porous fibrous insulations. Journal of alloys and Compounds, 657, 684–690. doi: https://doi.org/10.1016/j.jallcom.2015.09.099
- Datta, S., Das, S. (2005). A new high temperature resistant glass-ceramic coating for gas turbine engine components. Bulletin of Materials Science, 28 (7), 689–696. doi: https://doi.org/10.1007/bf02708539
- Kashin, D. S., Dergacheva, P. E., Stekhov, P. A. (2018). Heat resistant slurry coatings (review). Proceedings of VIAM, 5, 64–75. doi: https://doi.org/10.18577/2307-6046-2018-0-5-64-75
- Denisova, V. S., Lonskii, S. L., Kurshev, E. V., Malinina, G. A. (2019). Investigation of structure formation of reaction cured coatings by scanning electron microscopy. Proceedings of VIAM, 4, 76–87. doi: https://doi.org/10.18577/2307-6046-2019-0-4-76-87
- Denisova, V. S., Kurshev, E. V., Lonsky, S. L., Vlasova, O. V. (2020). Morphology and structure features of heat-resistant reactive for protection of heat-resistant nickel alloys. Proceedings of VIAM, 45, 54–61. doi: https://doi.org/10.18577/2307-6046-2020-0-45-54-61
- Donald, I. W., Mallinson, P. M., Metcalfe, B. L., Gerrard, L. A., Fernie, J. A. (2011). Recent developments in the preparation, characterization and applications of glass- and glass–ceramic-to-metal seals and coatings. Journal of Materials Science, 46 (7), 1975–2000. doi: https://doi.org/10.1007/s10853-010-5095-y
- Agüero, A., Muelas, R., Pastor, A., Osgerby, S. (2005). Long exposure steam oxidation testing and mechanical properties of slurry aluminide coatings for steam turbine components. Surface and Coatings Technology, 200 (5-6), 1219–1224. doi: https://doi.org/10.1016/j.surfcoat.2005.07.080
- Karasik, E., Marchan, R., Gorulya, N. (2019). Protective heat resistant coating for Inconel 718 additively manufactured parts. Proceedings of the International Astronautical Congress, IAC.
- Solncev, S. S., Shvagireva, V. V., Isaeva, N. V., Solovyeva, G. A. (2014). High temperature coating for protection of high-strength complex alloyed of nickel alloys of high-temperature gas corrosion. Proceedings of VIAM, 6, 4. doi: https://doi.org/10.18577/2307-6046-2014-0-6-4-4
- Goleus, V. I. (2017). Properties of borosilicate glass frit as a basis for obtaining glass-enamel coatings. Voprosy Khimii i Khimicheskoi Tekhnologii, 3, 47–52. Available at: http://oaji.net/articles/2017/1954-1500365372.pdf
- Lopes, S. C., Pagnano, V. O., Rollo, J. M. D. de A., Leal, M. B., Bezzon, O. L. (2009). Correlation between metal-ceramic bond strength and coefficient of linear thermal expansion difference. Journal of Applied Oral Science, 17 (2), 122–128. doi: https://doi.org/10.1590/s1678-77572009000200010
- Karasik, E. V., Hordieiev, Y. S. (2020). Calculation of thermal expansion, glass transition temperature and glass density in the system RO–Al2O3–B2O3–SiO2 (where RO=BaO, SrO, CaO, MgO, ZnO). Voprosy Khimii i Khimicheskoi Tekhnologii, 6, 69–74. doi: https://doi.org/10.32434/0321-4095-2020-133-6-69-74
- Hordieiev, Y. S., Karasik, E. V., Amelina, А. A. (2021). Properties of glasses in the system BaO–B2O3–SiO2–xAl2O3 (x=0; 5; 10 mol.%). Voprosy Khimii i Khimicheskoi Tekhnologii, 3, 83–89. doi: https://doi.org/10.32434/0321-4095-2021-136-3-83-89
- Goleus, V. I., Shul’ga, T. F. (2010). Calculation of the resistivity of silicate and borosilicate glasses as a function of their composition and temperature. Glass Physics and Chemistry, 36 (5), 575–578. doi: https://doi.org/10.1134/s1087659610050068
Downloads
Published
How to Cite
Issue
Section
License
Copyright (c) 2021 Elena Karasik, Yurii Hordieiev
This work is licensed under a Creative Commons Attribution 4.0 International License.
The consolidation and conditions for the transfer of copyright (identification of authorship) is carried out in the License Agreement. In particular, the authors reserve the right to the authorship of their manuscript and transfer the first publication of this work to the journal under the terms of the Creative Commons CC BY license. At the same time, they have the right to conclude on their own additional agreements concerning the non-exclusive distribution of the work in the form in which it was published by this journal, but provided that the link to the first publication of the article in this journal is preserved.
A license agreement is a document in which the author warrants that he/she owns all copyright for the work (manuscript, article, etc.).
The authors, signing the License Agreement with TECHNOLOGY CENTER PC, have all rights to the further use of their work, provided that they link to our edition in which the work was published.
According to the terms of the License Agreement, the Publisher TECHNOLOGY CENTER PC does not take away your copyrights and receives permission from the authors to use and dissemination of the publication through the world's scientific resources (own electronic resources, scientometric databases, repositories, libraries, etc.).
In the absence of a signed License Agreement or in the absence of this agreement of identifiers allowing to identify the identity of the author, the editors have no right to work with the manuscript.
It is important to remember that there is another type of agreement between authors and publishers – when copyright is transferred from the authors to the publisher. In this case, the authors lose ownership of their work and may not use it in any way.